PETG settings for the Adventurer 5M
Print PETG at 235°C nozzle and 60°C bed on the Flashforge Adventurer 5M.Settings below cover 4 nozzle sizes (0.25mm, 0.4mm, 0.6mm, 0.8mm).
Recommended settings (0.4 mm brass nozzle)
Nozzle temp235°C220–250°C range
Bed temp60°C55–70°C range
Fan speed100%Min 0%
Print speed60 mm/sStarting point
Retraction0.5 mmAt 40 mm/s
Nozzle0.4 mmbrass
Source: Official profile. ✓ Verified against official profile.
Imports directly into OrcaSlicer via File → Import → Import Configs
All nozzle sizes
0.25 mm nozzle
| Filament | Nozzle temp | Bed temp | Fan | Speed | Retraction | Source |
|---|---|---|---|---|---|---|
| Flashforge HS PETG Flashforge PETG Basic · Flashforge PETG Pro · Flashforge PETG Transparent | 235°C 220–250°C | 60°C 55–70°C | 100% /0% | 60 mm/s | 0.5 mm @ 40 mm/s | Official profile |
0.4 mm nozzle
| Filament | Nozzle temp | Bed temp | Fan | Speed | Retraction | Source |
|---|---|---|---|---|---|---|
| Flashforge HS PETG Flashforge PETG Basic · Flashforge PETG Pro · Flashforge PETG Transparent · Flashforge PETG-CF | 235°C 220–250°C | 60°C 55–70°C | 100% /0% | 60 mm/s | 0.5 mm @ 40 mm/s | Official profile |
0.6 mm nozzle
| Filament | Nozzle temp | Bed temp | Fan | Speed | Retraction | Source |
|---|---|---|---|---|---|---|
| Flashforge HS PETG Flashforge PETG Basic · Flashforge PETG Pro · Flashforge PETG Transparent · Flashforge PETG-CF | 235°C 220–250°C | 60°C 55–70°C | 100% /0% | 60 mm/s | 0.5 mm @ 40 mm/s | Official profile |
0.8 mm nozzle
| Filament | Nozzle temp | Bed temp | Fan | Speed | Retraction | Source |
|---|---|---|---|---|---|---|
| Flashforge HS PETG Flashforge PETG Basic · Flashforge PETG Pro · Flashforge PETG Transparent · Flashforge PETG-CF | 235°C 220–250°C | 60°C 55–70°C | 100% /0% | 60 mm/s | 0.5 mm @ 40 mm/s | Official profile |
Tips for printing PETG on the Flashforge Adventurer 5M
- PETG is hygroscopic — dry your filament before printing if stored openly for more than a week.
- Reduce fan speed to 25–50% for better layer adhesion. Too much cooling causes layer delamination.
- Use a higher first-layer height (0.25–0.3 mm) and reduce first-layer speed for better adhesion.
- PETG sticks aggressively to PEI — use a thin layer of glue stick or hairspray as release agent.