Flashforge › Adventurer 5M

PLA settings for the Adventurer 5M

Print PLA at 215°C nozzle and 60°C bed on the Flashforge Adventurer 5M.Settings below cover 4 nozzle sizes (0.25mm, 0.4mm, 0.6mm, 0.8mm).

Recommended settings (0.4 mm brass nozzle)

Nozzle temp215°C190–230°C range
Bed temp60°C55–70°C range
Fan speed100%Min 0%
Print speed60 mm/sStarting point
Retraction0.5 mmAt 40 mm/s
Nozzle0.4 mmbrass

Source: Official profile. ✓ Verified against official profile.

Imports directly into OrcaSlicer via File → Import → Import Configs

All nozzle sizes

0.25 mm nozzle

FilamentNozzle tempBed tempFanSpeedRetractionSource
Flashforge HS PLA
Flashforge
215°C
190–230°C
45°C
40–55°C
100% /0%60 mm/s0.5 mm @ 40 mm/sOfficial profile
Flashforge PLA Basic
Flashforge PLA Color Change · Flashforge PLA Galaxy · Flashforge PLA Luminous · Flashforge PLA Matte · Flashforge PLA Metal · Flashforge PLA Pro · Flashforge PLA Silk · Flashforge PLA Sparkle
215°C
190–230°C
60°C
55–70°C
100% /0%60 mm/s0.5 mm @ 40 mm/sOfficial profile

0.4 mm nozzle

FilamentNozzle tempBed tempFanSpeedRetractionSource
Flashforge HS PLA
Flashforge PLA Basic · Flashforge PLA Color Change · Flashforge PLA Galaxy · Flashforge PLA Luminous · Flashforge PLA Matte · Flashforge PLA Metal · Flashforge PLA Pro · Flashforge PLA Silk
215°C
190–230°C
60°C
55–70°C
100% /0%60 mm/s0.5 mm @ 40 mm/sOfficial profile

0.6 mm nozzle

FilamentNozzle tempBed tempFanSpeedRetractionSource
Flashforge HS PLA
Flashforge PLA Basic · Flashforge PLA Color Change · Flashforge PLA Galaxy · Flashforge PLA Luminous · Flashforge PLA Matte · Flashforge PLA Metal · Flashforge PLA Pro · Flashforge PLA Silk
215°C
190–230°C
60°C
55–70°C
100% /0%60 mm/s0.5 mm @ 40 mm/sOfficial profile

0.8 mm nozzle

FilamentNozzle tempBed tempFanSpeedRetractionSource
Flashforge HS PLA
Flashforge PLA Basic · Flashforge PLA Color Change · Flashforge PLA Galaxy · Flashforge PLA Luminous · Flashforge PLA Matte · Flashforge PLA Metal · Flashforge PLA Pro · Flashforge PLA Silk
215°C
190–230°C
60°C
55–70°C
100% /0%60 mm/s0.5 mm @ 40 mm/sOfficial profile

Tips for printing PLA on the Flashforge Adventurer 5M

  • PLA is the easiest filament to print. Start with the recommended 215°C nozzle temperature and adjust by ±5°C based on under/over-extrusion.
  • Keep fan speed at 100% for best layer adhesion and bridging performance.
  • Bed adhesion is excellent with a clean PEI sheet — no glue stick needed.
  • Lower print speed (40–50 mm/s) for detailed parts; increase to 80+ mm/s for drafts.