PETG settings for the SV06 Plus
Print PETG at 235°C nozzle and 80°C bed on the SV06 Plus.Fan speed 50%, retraction 0.5mm, print speed 40mm/s.
Recommended settings (0.4 mm brass nozzle)
Nozzle temp235°C220–250°C range
Bed temp80°C75–90°C range
Fan speed50%Min 20%
Print speed40 mm/sStarting point
Retraction0.5 mmAt 35 mm/s
Nozzle0.4 mmbrass
Source: Derived. Based on manufacturer specifications.
Imports directly into OrcaSlicer via File → Import → Import Configs
0.4 mm nozzle
| Filament | Nozzle temp | Bed temp | Fan | Speed | Retraction | Source |
|---|---|---|---|---|---|---|
| PETG Generic | 235°C 220–250°C | 80°C 75–90°C | 50% /20% | 40 mm/s | 0.5 mm @ 35 mm/s | Derived |
Tips for printing PETG on the SV06 Plus
- PETG is hygroscopic — dry your filament before printing if stored openly for more than a week.
- Reduce fan speed to 25–50% for better layer adhesion. Too much cooling causes layer delamination.
- Use a higher first-layer height (0.25–0.3 mm) and reduce first-layer speed for better adhesion.
- PETG sticks aggressively to PEI — use a thin layer of glue stick or hairspray as release agent.