Flashforge › Guider4 Pro

PETG settings for the Guider4 Pro

Print PETG at 235°C nozzle and 80°C bed on the Flashforge Guider4 Pro.Settings below cover 3 nozzle sizes (0.25mm, 0.4mm, 0.6mm).

Recommended settings (0.4 mm brass nozzle)

Nozzle temp235°C220–250°C range
Bed temp80°C75–90°C range
Fan speed100%Min 0%
Print speed60 mm/sStarting point
Retraction0.5 mmAt 40 mm/s
Nozzle0.4 mmbrass

Source: Official profile. ✓ Verified against official profile.

Imports directly into OrcaSlicer via File → Import → Import Configs

All nozzle sizes

0.25 mm nozzle

FilamentNozzle tempBed tempFanSpeedRetractionSource
Flashforge HS PETG
Flashforge PETG Pro · Flashforge PETG Transparent
235°C
220–250°C
80°C
75–90°C
100% /0%60 mm/s0.5 mm @ 40 mm/sOfficial profile

0.4 mm nozzle

FilamentNozzle tempBed tempFanSpeedRetractionSource
Flashforge HS PETG
Flashforge PETG Pro · Flashforge PETG Transparent · Flashforge PETG-CF
235°C
220–250°C
80°C
75–90°C
100% /0%60 mm/s0.5 mm @ 40 mm/sOfficial profile

0.6 mm nozzle

FilamentNozzle tempBed tempFanSpeedRetractionSource
Flashforge HS PETG
Flashforge PETG Pro · Flashforge PETG Transparent · Flashforge PETG-CF
235°C
220–250°C
80°C
75–90°C
65% /30%60 mm/s0.5 mm @ 40 mm/sOfficial profile

Tips for printing PETG on the Flashforge Guider4 Pro

  • PETG is hygroscopic — dry your filament before printing if stored openly for more than a week.
  • Reduce fan speed to 25–50% for better layer adhesion. Too much cooling causes layer delamination.
  • Use a higher first-layer height (0.25–0.3 mm) and reduce first-layer speed for better adhesion.
  • PETG sticks aggressively to PEI — use a thin layer of glue stick or hairspray as release agent.