Inland Filament Settings

Inland is Micro Center's house brand filament — consistently reliable, with one of the best cost-per-spool ratios of any US-available filament when purchased in-store. These are the recommended slicer settings for Inland PLA, PETG, ABS, TPU, and Matte PLA on any FDM printer.

Budget — best US in-store valuePLA · PETG · ABS · TPU · MatteMicro Center only

Settings by material

PLA

Nozzle temp195–220°CStart at 205°C
Bed temp55–65°CStart at 60°C
Retraction1–2 mm (DD) / 4–6 mm (Bowden)45 mm/s
Fan100%
Print speed50–80 mm/s
Bed surfaceSmooth PEI, glass, BuildTak

Inland PLA is the Micro Center house brand — one of the most affordable quality filaments in the US. Prints reliably at 200–210°C on most printers. White and black colors are particularly consistent. Diameter tolerance is good for the price (±0.03 mm).

PLA+ (Tough PLA)

Nozzle temp210–230°CStart at 220°C
Bed temp60–70°CStart at 65°C
Retraction1–2 mm (DD) / 5–6 mm (Bowden)45 mm/s
Fan100%
Print speed45–70 mm/s
Bed surfaceSmooth PEI, glass

Inland Tough PLA is their PLA+ variant. 10°C warmer than their standard PLA for good layer bonding. More impact resistant and less brittle — good for functional parts at standard PLA ease of printing.

PETG

Nozzle temp230–250°CStart at 240°C
Bed temp70–85°CStart at 80°C
Retraction1–2 mm (DD) / 5–7 mm (Bowden)25 mm/s
Fan30–50%
Print speed35–55 mm/s
Bed surfaceTextured PEI, glass + glue

Inland PETG is straightforward at 240°C on most printers. Use combing mode to minimize stringing. Keep fan at 30–50% — lower than PLA for good interlayer bonding. Textured PEI is preferred; smooth PEI will bond aggressively and can damage the surface.

ABS

Nozzle temp230–250°CStart at 240°C
Bed temp100–110°CStart at 105°C
Retraction1–2 mm (DD) / 5–7 mm (Bowden)30 mm/s
Fan0%
Print speed40–60 mm/s
Bed surfaceSmooth PEI + ABS slurry, Kapton tape

Inland ABS follows standard ABS requirements — enclosure is essential for large parts. Disable fan completely. Use an ABS slurry (ABS in acetone) on smooth PEI. Inland ABS is known for good layer adhesion when printed correctly.

TPU 95A

Nozzle temp220–240°CStart at 230°C
Bed temp40–60°CStart at 50°C
Retraction0–1 mm (DD only)20 mm/s
Fan100%
Print speed20–30 mm/s
Bed surfaceSmooth PEI, glass

Inland TPU 95A requires direct drive. Print at 20–25 mm/s maximum. Zero or minimal retraction (0.5 mm) to prevent grinding and clogs. Good flexibility and durability for the price — a popular choice for Micro Center shoppers wanting to try flexible filament.

PLA Matte

Nozzle temp200–220°CStart at 210°C
Bed temp55–65°CStart at 60°C
Retraction1–2 mm (DD) / 4–6 mm (Bowden)40 mm/s
Fan100%
Print speed40–70 mm/s
Bed surfaceSmooth PEI, glass

Inland Matte PLA is a popular value option. Matte surfaces hide layer lines better than standard PLA. Same settings as regular PLA with no special adjustments needed. The matte finish requires slightly slower outer wall speeds (40–50 mm/s) for the best texture.

Inland quick tips

  • Print cooler than average: Inland PLA runs 5–10°C cooler than many brands. Start at 200–205°C rather than the typical 210–215°C default. Too much heat causes stringing and blobs before you will see underextrusion.
  • In-store vs. online pricing: Inland's value proposition is in-store pricing at Micro Center. Online orders include shipping costs that significantly reduce the price advantage. If you're near a Micro Center, pick up spools in person.
  • Matte PLA for clean models: Inland Matte PLA hides layer lines better than glossy PLA. Slow outer walls to 40–50 mm/s for the best matte texture. No slicer changes needed beyond outer wall speed.
  • Store filament properly: Inland vacuum-seals their filament but the bags are not resealable. Transfer to airtight containers with desiccant — especially important in humid climates for PETG and ABS.
  • ABS: enclosure is not optional: Inland ABS will warp on open-frame printers for anything wider than ~50 mm. Use ASA or PETG as a warping-resistant substitute if you don't have an enclosure.