PLA settings for the Sidewinder X3 Pro
Print PLA at 215°C nozzle and 60°C bed on the Artillery Sidewinder X3 Pro.Fan speed 80%, retraction 1.3mm, print speed 60mm/s.
Recommended settings (0.4 mm brass nozzle)
Nozzle temp215°C190–230°C range
Bed temp60°C55–70°C range
Fan speed80%Min 60%
Print speed60 mm/sStarting point
Retraction1.3 mmAt 40 mm/s
Nozzle0.4 mmbrass
Source: Official profile. ✓ Verified against official profile.
Imports directly into OrcaSlicer via File → Import → Import Configs
0.4 mm nozzle
| Filament | Nozzle temp | Bed temp | Fan | Speed | Retraction | Source |
|---|---|---|---|---|---|---|
| Artillery PLA Basic Artillery PLA Matte · Artillery PLA Silk | 215°C 190–230°C | 60°C 55–70°C | 80% /60% | 60 mm/s | 1.3 mm @ 40 mm/s | Official profile |
| Artillery PLA Tough Artillery | 215°C 190–230°C | 65°C 60–75°C | 80% /60% | 60 mm/s | 1.3 mm @ 40 mm/s | Official profile |
Tips for printing PLA on the Artillery Sidewinder X3 Pro
- PLA is the easiest filament to print. Start with the recommended 215°C nozzle temperature and adjust by ±5°C based on under/over-extrusion.
- Keep fan speed at 100% for best layer adhesion and bridging performance.
- Bed adhesion is excellent with a clean PEI sheet — no glue stick needed.
- Lower print speed (40–50 mm/s) for detailed parts; increase to 80+ mm/s for drafts.